Buy From China Factory!

Superalloy Castings Parts Cobalt Alloy Castings Parts Nozzle With Wax Lost

Contact Supplier
Product Details
Brand Name:Eternal Bliss
Model Number:EB9064
Certification:ISO9001-2008
Price:USD100~ USD150/kg
Payment Terms:by T/T or L/C, Western Union
Supply Ability:2000 tons per year
Delivery Time:It depends on the quantity to be ordered.
Company Profile
Active Member
Business Type: Manufacturer Distributor/Wholesaler Agent Importer Exporter Trading Company Seller
Contact Person: Juliet Zhu
Officials: 1099 Xinhua Road,214104, Xishan District, Wuxi, Jiangsu,China
Item Description

Cobalts Alloy Castings Parts Nozzle with Wax Lost Process EB9064 We produce High Temperature Superalloy Castings Parts with centrifugal cast process, ...

More 

Cobalt Alloy Castings